Optimizing Whims Parameters for Kaolin Ore Beneficiation from the Mine of Tamazert Using Box–Behnken Design

Authors

  • Mohammed Laraba University of Tebessa

DOI:

https://doi.org/10.59150/ibgm2201a13

Keywords:

Tamazert kaolin ore; Fe2O3; WHIMS; RSM; Box–Behnken Design.

Abstract

This research aimed to enhance the quality of kaolin ore extracted from the Tamazert mine in Northeast Algeria through wet high-intensity magnetic separation (WHIMS), specifically targeting the removal of coloring impurities. The experiment involved examining various parameters that could potentially influence the separation process. To systematically analyze these factors, a response surface methodology (RSM) was employed, utilizing the Box-Behnken design. This design allows for efficient exploration of multiple variables within a limited number of experimental runs, facilitating the identification of optimal conditions for the separation process. For the characterization, multiple analytical techniques, including X-ray fluorescence (XRF), X-ray diffraction (XRD), and Scanning Electron Microscopy coupled with Energy Dispersive X-ray Spectroscopy (SEM-EDX), were employed. The obtained results of characterization reveal that the kaolin from Tamazert mine is an alumino-silicate containing kaolinite with hematite (Fe2O3: 4.7%) as the main impurity and titanium with low content (TiO2: 0.08%). The statistical analysis indicated that intensity (I) was the most significant and influential factor to eliminate iron from Tamazert kaolin ore, followed by the ball sizes (BS) of the matrix and grain sizes (GS) of particles. The optimization approach was determined to be I = 2T, BS = 20 mm, and GS = 10 μm to achieve the maximum content target of 5.77% Fe with a yield of 94.60%. Overall, the study demonstrated that WHIMS could effectively remove iron impurities from Tamazert kaolin ore and improve its quality to be used in several applications.

Downloads

Published

2026-06-30

Issue

Section

Articles